Banner
Home > News Center > Content
What are the reasons for the streaks in stainless steel fittings?
- 2021-04-15-

During the entire operation of stainless steel castings, you will notice some streaks. As a stainless steel casting manufacturer in Guangdong, let me take everyone to learn about the reasons for the streaks of stainless steel castings to facilitate better operation.

The two metal streams of stainless steel castings are not the same as the signs of residues that fill the cavity and stay, which may be caused by such conditions. The mold temperature is low. For example, the mold temperature of the zinc alloy material is less than150℃, the mold temperature of aluminum alloy profile is less than180℃, it is easy to cause such shortcomings.

The filling rate of stainless steel castings is too fast, and it is very easy to produce such streaks, or if the architectural coating is used too much, the streaks will also occur. All in all, the appearance of stripes represents this batch of stainless steel casting products, because it has no beautiful appearance design, which jeopardizes the aesthetic standards of stainless steel castings.

All normal conditions will be avoided Countermeasures for stainless steel castings, if you want to make the quality of stainless steel castings better, you must choose an appropriate casting method. There is also the selection of raw materials, followed by gaining a lot of work experience in daily work. This name seems to be valid, and it also helps everyone find a way to manufacture castings. The cross-section and position, shape and size of the inner gate can be Decide the fluidity rate, fluidity direction and flow of the metal material liquid, and have the Important contact. Thin inner gate, high metal material liquid movement, is beneficial to filling thin walls and various parts, so that the appearance of the casting is clear, and the speed must be adjusted appropriately. Adjusting the mold temperature and adding overflow grooves can also avoid this phenomenon; in order to better avoid streaks, the operation of architectural coatings is thin and uniform.